SmCo magnets, are composed of Samarium, Cobalt, and a few transition metals. SmCo magnets are high performance, low temperature coefficient rare earth permanent magnets, and could keep their performance under the maximum working temperature up to 350 degree centigrade.
Manufacturing Process
Samarium, Cobalt, and a few transition metals will be made into the
SmCo powder, then fine SmCo powder will be compacted in a die and
sintered, fusing the powder into a solid material. There are 2 forms of
pressing: die pressing and isostatic pressing. Sintered parts normally
need some finish machining in order to meet final tolerances.
Machining & Tolerance
Generally, SmCo magnets must be machined using diamond-grinding
techniques. Sometimes, machining operations may be performed on SmCo
materials using carbide tools, but surface finishes thus obtained may be
less than optimal.
The Standard tolerances for SmCo magnets are +/- 0.1mm for ground
dimensions, but sticter tolerances are possible if specially required.
Surface treatments
The corrosion resistance of SmCo magnets is considered good. Although
Surface coating or plating is not generally required for SmCo magnets,
all kinds of surface coating are also available, like Nickel, Zn,
Ni-Cu-Ni, Gold, Silver, Sn,Chrome, ABS coating, Rubber coating,
PTFE(Telfon) coating, stainless steel case and Epoxy coating etc.
Magnetizing & Packing
SmCo magnets require extremely high magnetizing fields, and can be
magnetized in any direction as long as it is aligned properly. In some
instances multiple pole magnetization is possible with special fixtures.
All SmCo magnets are anisotropic, and can only be magnetized in the
orientation direction, so particular consideration must be given to this
when designing complex assemblies, if it is intended to magnetize after
installation.
SmCo magnets are mechanically weak, but magnetically very strong. They
should be packed properly in order to help user to handle them safely.
Magnetic Properties of SmCo Magnets:
Grade | Residual Induction | Coercive Force | Intrinsic Coercive Force | Maximum Energy Product | Maximum Working Temperature | |
Br | Hcb | Hcj | (BH)max | Tw | ||
mT | kA/m | kA/m | kJ/m3 | |||
[kGs] | [kOe] | [kOe] | [MGOe] | |||
SmCo5 | YX18 | 820-920 | 639-756 | 1194-1751 | 127-159 | 250° |
[8.2-9.2] | [8-9.5] | [15-22] | [16-20] | |||
YX20 | 870-950 | 639-756 | 1194-1751 | 143-175 | ||
[8.7-9.5] | [8-9.5] | [15-22] | [18-22] | |||
YX22 | 930-1000 | 660-772 | 1194-1751 | 159-191 | ||
[9.3-1.0] | [8.3-9.7] | [15-22] | [20-24] | |||
YX24 | 960-1040 | 660-780 | 1194-1751 | 175-207 | ||
[9.6-10.4] | [8.3-9.8] | [15-22] | [22-26] | |||
Sm2Co17 | YXS24M | 960-1040 | 318-772 | 398-955 | 175-207 | 350° |
[9.6-10.4] | [4-9.7] | [5-12] | [22-26] | |||
YXS24 | 960-1040 | 660-780 | ≥1194 | 175-207 | ||
[9.6-10.4] | [8.3-9.8] | [≥15] | [22-26] | |||
YXS24H | 960-1040 | 660-780 | ≥1592 | 175-207 | ||
[9.6-10.4] | [8.3-9.8] | [≥20] | [22-26] | |||
YXS26M | 1170-1220 | 318-796 | 398-955 | 191-223 | ||
[10-10.7] | [4-10] | [5-12] | [25-28] | |||
YXS26 | 1170-1220 | 677-820 | ≥1194 | 191-223 | ||
[10-10.7] | [8.5-10.3] | [≥15] | [25-28] | |||
YXS26H | 1170-1220 | 677-820 | ≥1592 | 191-223 | ||
[10-10.7] | [8.5-10.3] | [≥20] | [25-28] | |||
YXS28M | 1040-1110 | 318-796 | 398-955 | 207-239 | ||
[10.4-11] | [4-10] | [5-12] | [26-30] | |||
YXS28 | 1040-1110 | 677-820 | ≥1194 | 207-239 | ||
[10.4-11] | [8.5-10.3] | [≥15] | [26-30] | |||
YXS28H | 1040-1110 | 677-820 | ≥1592 | 207-239 | ||
[10.4-11] | [8.5-10.3] | [≥20] | [26-30] | |||
YXS30M | 1070-1120 | 318-796 | 398-955 | 223-247 | ||
[10.7-11.2] | [4-10] | [5-12] | [28-31] | |||
YXS30 | 1070-1120 | 677-820 | ≥1194 | 223-247 | ||
[10.7-11.2] | [8.5-10.3] | [≥15] | [28-31] | |||
YXS32M | 1090-1150 | 318-796 | 398-955 | 238-262 | ||
[10.9-11.5] | [4-10] | [5-12] | [29-32] | |||
YXS32 | 1090-1150 | 677-820 | ≥1353 | 238-262 | ||
[10.9-11.5] | [8.5-10.3] | [≥12] | [29-32] | |||
Low Temp Coeff Sm2Co17 | YXL22LT | 930-1000 | 677-756 | ≥1194 | 159-191 | 350° |
[9.3-10] | [8.5-9.5] | [≥15] | [20-24] | |||
YXL24LT | 960-1040 | 677-756 | ≥1194 | 175-207 | ||
[9.6-10.4] | [8.5-9.5] | [≥15] | [22-26] | |||
YXL26LT | 1000-1070 | 677-812 | ≥1433 | 191-223 | ||
[10-10.7] | [8.5-10.2] | [≥18] | [25-28] |
Physical Properties of SmCo Magnets:
Grade | Modulus of elasticy | Ultimate tensile strength | Density | Electrical Resistivity | Curie temperature | Recoil permeability | Temp.Coeff.of Br |
SmCo5 | 23 x 106 psi | 6 x 103 psi | 8.2 g/cm3 | 5 µ-ohm-cm/cm2 | 750-770℃ | 1.05 | From -0.043 to -0.045% / ℃ |
Sm2Co17 | 17 x 106 psi | 5 x 103 psi | 8.4 g/cm3 | 86 µ-ohm-cm/cm2 | 825-850℃ | 1.05 | From -0.03 to -0.032% / ℃ |